Polymer Property : Boiling Point = 82.4 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Boiling Point 28.0 °C
82.4 °F
Iso-Pentane
LG Chemical IP-20
Structure & Characteristics: C5H10. A ring-structured saturated hydrocarbon. Present in naphtha pyrolysis oil and is obtained by distillation followed by isolation of n-pentane extraction remnants o..
Boiling Point 28.0 °C
82.4 °F
Iso-Pentane
LG Chemical IP-40
Structure & Characteristics: C5H10. A ring-structured saturated hydrocarbon. Present in naphtha pyrolysis oil and is obtained by distillation followed by isolation of n-pentane extraction remnants o..
Boiling Point 28.0 °C
82.4 °F
LG Chemical i-Pentane
Structure & Characteristics: C5H10. A ring-structured saturated hydrocarbon. Present in naphtha pyrolysis oil and is obtained by distillation followed by isolation of n-pentane extraction remnants o..