Thermal Properties Metric English Comments
Boiling Point 242 °C
468 °F
at 760 mmHg
LyondellBasell Glycol Ether DBA Diethylene glycol butyl ether acetate
Information provided by Lyondell.
Boiling Point 242 °C
468 °F
at 760 mmHg
LyondellBasell Propylene Carbonate
Information provided by Lyondell.
Boiling Point 242 °C
468 °F
Initial; ASTM D86
ExxonMobil Solvesso™ 200 ND Aromatic Fluid
Appearance: Transparent - Slight Yellow LiquidAvailability: Africa & Middle East, Europe, Asia Pacific, Central America, North America and South AmericaInformation provided by ExxonMobil
Boiling Point 242 °C
468 °F
BASF 2-Pyrrolidone Water Blend
Formula: C4H7NOCAS: 7732-18-5Description: Pyrrolidone is a colorless to yellow liquid, with a faint amine-like odor. It is miscible in water.Synonyms: 2P water blend, Pyrrolidone, 2-Pyrrolidinone, 2..