Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 216 °C | 421 °F | 1013 mbar |
BASF 2- Ethylhexyl Acrylate Formula: C11H20O2CAS: 203-080-7Description: Acrylic ester for manufacturing polymers and for use as a feedstock for syntheses. Applications: 2-Ethylhexyl acrylate forms homopolymers and copolymers. .. |
|||
Boiling Point | 216 °C | 421 °F | |