Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 47.0 - 48.0 °C | 117 - 118 °F | |
BASF Propionaldehyde Formula: C3H6OCAS: 123-38-6Description: Propionaldehyde is a colorless liquid, with a pungent odor. It is miscible in water in all proportions and is soluble in other organic solvents.Synonyms: Prop.. |