Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 79.0 °C | 174 °F | of Solvent |
3M Novec™ 2708 Electronic Grade Coating 3M™ Novec™ 2708 Electronic Grade Coating is designed for the protection of printed circuit boards and electronic components. It is a low viscosity solution of a 8 wt% fluorochemical acrylic polyme.. |