Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 64.0 °C | 147 °F | |
BASF Propargyl Chloride 35% Solution in Toluene Formula: C3H3ClCAS: 624-65-7Description: Propargyl Chloride is a 35% solution in Toluene. It is a colorless to yellow liquid, with a faint odor. It is sparingly soluble with water.Synonyms: 3 Chlor.. |