Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 221 °C | 430 °F | Initial; ASTM 1078 |
ExxonMobil Exxsol™ D220/240 Dearomatized Fluid Availability: Africa & Middle East, Europe, Central America and South America Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil |
|||
Boiling Point | 221 °C | 430 °F | |
BASF N3-Amine 3-(2-aminoethylamino)propylamine Formula: C8H22N4CAS: 13531-52-7Description: N3-Amine is a colorless to yellow liquid with an amine-like odor. It is miscible in water.Synonyms: N-(2-Amino)-1,3-diaminopropane, N-(3-Aminopropyl)-1,2.. |