Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | <= 215 °C | <= 419 °F | End |
Kazanorgsintez E-13 Petroleum Resin Production Method: Obtained as a by-product in the process of hydrocarbon gas pyrolysis on ethylene production plants. Application: Feedstock for production of motor fuel, solvents and aromatic .. |
|||
Boiling Point | 215 °C | 419 °F | |
Solvay Specialty Polymers Galden® LLS215 PFPE VPS Fluid Galden® LS and HS grades are specifically recommended for vapor phase soldering.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of servic.. |
|||
Boiling Point | 215 °C | 419 °F | |
Dow Corning 704 DIFFUSION PUMP FLUID A clear, tetramethyltetra-phenyltrisiloxane, single-component fluid for high vacuums of 10-7 to 10-8 torr range (untrapped) and 10-11 (trapped).Information provided by Dow Corning |
|||
Boiling Point | 215 °C @Pressure 0.101 MPa |
419 °F @Pressure 14.7 psi |
|
3M Fluorinert™ FC-70 Electronic Liquid Fluorinert™ Liquid FC-70 a non-conductive, thermally and chemically stable liquid that offers a high boiling point (215 deg C), it is ideal for many electronics single and two phase heat transfer a.. |
|||
Boiling Point | 215 °C | 419 °F | |
BASF Tributylamine Formula: C12H27NCAS: 102-82-9Description: Tributylamine is a colorless liquid with an amine-like odor. Synonyms: Tri-n-butylamine, 1-Butanamine,N,N-dibutyl, N,N-Dibutylbutan-1-aminApplications: Inte.. |