Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | >= 200 °C | >= 392 °F | |
Hong Kun Group AO 1135 Antioxidant This product is phenols antioxidant, applicable to the occasion that there are liquor, latex, soliquoid and mixture,especially applicable to polyols and polyurethane.it has excellent effect in anti-.. |
|||
Boiling Point | 200 °C | 392 °F | at 760 mmHg |
LyondellBasell DPMA Dipropylene glycol methyl ether acetate Information provided by Lyondell. |
|||
Boiling Point | 200 °C | 392 °F | |
Solvay Chemicals ANTAROX® BL-225 Wetting agent as suspension additivesHS No.: 34021300 /CAS-No.: 68603-25–8 Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & Electrical Appl.. |
|||
Boiling Point | 200 °C | 392 °F | |
Solvay Specialty Polymers Galden® HT200 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
Boiling Point | 200 °C | 392 °F | |
Solvay Specialty Polymers Galden® LS200 PFPE VPS Fluid Galden® LS and HS grades are specifically recommended for vapor phase soldering.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of servic.. |
|||
Boiling Point | 200 °C | 392 °F | |
Solvay ANTAROX® BL 225 Surfactant Description: Biodegradable linear alcohol EO/PO. Low foaming non-ionic with excellent hard surface detergency combined to wetting properties. Soluble in water and most organic solvents except paraff.. |
|||
Boiling Point | >= 200 °C @Pressure 0.000667 MPa |
>= 392 °F @Pressure 0.0967 psi |
|
BASF Lupranate® 5100 Isocyanate Description: Lupranate® 5100 Isocyanate is an isocyanate blend of monomeric and polymeric MDI. Typical use is for flexible slab stock and molded Visco-Elastic memory foams.Information provided by B.. |
|||
Boiling Point | 200 - 202 °C | 392 - 396 °F | |
BASF 2-Phenylethylamine Formula: C8H11NCAS: 64-04-0Description: 2-Phenylethylamine is a colorless to yellow liquid with an amine-like odor. Synonyms: Phenylethylamin, Benzolethanamin, PhenylethylamineApplications: Intermed.. |