Polymer Property : Boiling Point = 148 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Boiling Point 148 °C
298 °F
LG Chemical Butyl Acrylate
Features: Low Color - Refining process are improved for produce the low color. Color is the main quality factor that influence the property of the final products. Low Acidity - Through the multistag..
Boiling Point 148 °C
298 °F
BASF Butyl Acrylate
Formula: C7H12O2CAS: 141-32-2Description: Acrylic acid ester, for manufacturing polymers and for use as a feedstock for syntheses.Applications: Butyl acrylate forms homopolymers and copolymers. Copo..