Polymer Property : Boiling Point = 104 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Boiling Point 104 °C
219 °F
Initial; ASTM D86
ExxonMobil Exxsol™ DSP100/120 Dearomatized Fluid
Availability: Africa & Middle East and Europe Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil
Boiling Point 104 °C
219 °F
ConocoPhillips 46 FC Fluid-D ISO
Description: Conoco FC Fluid-D is a premixed, ready-to-use fluid for hydraulic systems, such as those found in underground-mining equipment that operate where fire-hazard and other personnel safety ..
Boiling Point 104 - 108 °C
219 - 226 °F
BASF DMF-DM 1,1-Dimethoxy-N,N-dimethyl methanamine
Formula: C5H13NO2CAS: 4637-24-5Description: DMF-DMA is a colorless to yellow liquid, with an ether-like odor. In water is spontaneously decomposes and is soluble in organic solvents.Synonyms: DMF-D..
Boiling Point 104 °C
219 °F
BASF Glyoxal 40%
Formula: C2H2O2CAS: 107-22-2Description: Glyoxal is a colorless to yellow liquid, with a faint odor. It is also miscible with water.Synonyms: Glyoxaldehyde, Ethanedial, 1,2-Ethanedione, Diformyl, E..