Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 135 - 145 °C | 275 - 293 °F | |
Oceanchem Group Brominated Epoxy Oligomers-2 (BEP-2) Molecular Formula: (C36H32Br8O6)nCas No.: 68928-70-1Application: BEP-2 is a high molecular weight brominated epoxy polymeric flame retardant designed for a broad range of thermoplastic applications... |
|||
Softening Point | 129 - 145 °C | 264 - 293 °F | |
Beijing Ranger Chem SM-609R Solid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |