Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 124 - 132 °C | 255 - 270 °F | |
Beijing Ranger Chem 197 Solid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Softening Point | 110 - 132 °C | 230 - 270 °F | |
AdvanSource Biomaterials HydroMed™ D640 Permanently Lubricious Polyurethane Coating AdvanSource Biomaterials Corporation manufactures and markets hydrophilic high slip, high water absorptive, polyether hydrophilic polyurethanes designed for use as coatings of catheters, sutures, in.. |
|||
Softening Point | 110 - 132 °C | 230 - 270 °F | |
AdvanSource Biomaterials HydroSlip™ C Hydrophilic Polyether Aliphatic Polyurethane AdvanSource Biomaterials Corporation manufactures and markets thermoplastic elastomeric hydrogels under the tradename HydroThane™. HydroThane™ is a generic family of polyurethane hydrogels, with .. |