Softening Point 110 - 120 °C
230 - 248 °F
Oceanchem Group Brominated Epoxy Oligomers-1 (BEP-1)
Molecular Formula: (C36H32Br8O6)nCas No.: 68928-70-1Application: BEP-1 is used in ABS/HIPS etc.Information Provided by Oceanchem Group
Softening Point 100 - 120 °C
212 - 248 °F
Kazanorgsintez 158-125 Low Density Polyethylene Composite
Production Method: Produced from low density polyethylene grades 15803-020 and 15813-020. Application: Designed for production of sealing coatings on industrial items.Information Provided by Kaz..
Softening Point 105 - 120 °C
221 - 248 °F
Kazanorgsintez 158BK-15 Low Density Polyethylene Composite
Production Method: Produced from low density polyethylene grades 15803-020 and 15813-020. Application: Designed for production of sealing coatings on industrial items.Information Provided by Kaz..
Softening Point 100 - 120 °C
212 - 248 °F
Kazanorgsintez 158BK-20 Low Density Polyethylene Composite
Production Method: Produced from low density polyethylene grades 15803-020 and 15813-020. Application: Designed for production of sealing coatings on industrial items.Information Provided by Kaz..
Softening Point 100 - 120 °C
212 - 248 °F
flow beginning
Taiwan Sheen Soon Sheenthane® AH-591 TPU for Hotmelt Adhesive
Thermoplastic polyurethane elastomer for soft hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes..
Softening Point 100 - 120 °C
212 - 248 °F
flow beginning
Taiwan Sheen Soon Sheenthane® AH-701 TPU for Hotmelt Adhesive
Thermoplastic polyurethane elastomer for hotmelt adhesiveHydrolysis resistance gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. U..
Softening Point 100 - 120 °C
212 - 248 °F
flow beginning
Taiwan Sheen Soon Sheenthane® AH-780 TPU for Hotmelt Adhesive
Thermoplastic polyurethane elastomer for hotmelt adhesiveNon-yellowing, aliphatic gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized...
Softening Point 100 - 120 °C
212 - 248 °F
flow beginning
Taiwan Sheen Soon Sheenthane® AH-781 TPU for Hotmelt Adhesive
Thermoplastic polyurethane elastomer for hotmelt adhesiveNon-yellowing, aliphatic gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized...
Softening Point 100 - 120 °C
212 - 248 °F
flow beginning
Taiwan Sheen Soon Sheenthane® AH-571 TPU for Hotmelt Adhesive
Thermoplastic polyurethane elastomer for soft hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes..
Softening Point 115 - 120 °C
239 - 248 °F
MQSA 70 A
Lubrizol Advanced Materials PEARLBOND® 151 Linear Thermoplastic Polyurethane  (discontinued **)
PEARLBOND® 125/H is polycaprolactone-based thermoplastic polyurethane, supplied in form of colourless or slightly yellowish, translucid pellets, combining a low hardness with excellent low-temperat..