Polymer Property : Softening Point = 225 °F
Polymer Property :
Softening Point =
225 °F
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Softening Point
96.0
-
107
°C
205
-
225
°F
Beijing Ranger Chem SM-604R Solid Epoxy Resin
Information provided by Beijing Ranger Chemical Co.