Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 85.0 - 105 °C | 185 - 221 °F | flow beginning |
Taiwan Sheen Soon Sheenthane® AH-530 TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for soft hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes.. |
|||
Softening Point | 85.0 - 105 °C | 185 - 221 °F | flow beginning |
Taiwan Sheen Soon Sheenthane® AH-560 TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for soft hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes.. |
|||
Softening Point | 95.0 - 105 °C | 203 - 221 °F | |
Beijing Ranger Chem 195 Solid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |