Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 98.9 - 104 °C | 210 - 220 °F | |
Plaskolite Optix® DA Digital Acrylic Sheet Designed to provide optimal adhesion of UV curing inks without adhesion promoters, OPTIX DA is a continuously processed acrylic sheet specially formulated product for printing. OPTIX DA provides sup.. |