Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 90.0 - 100 °C | 194 - 212 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 110 Linear Thermoplastic Polyurethane
(discontinued **) PEARLBOND® 110 is a linear, aromatic polyurethane, supplied in form of white slightly yellowish pellets, which combines a high crystallization rate with a low thermoplasticity level.Applications: P.. |
|||
Softening Point | 90.0 - 100 °C | 194 - 212 °F | MQSA 70A |
Lubrizol Advanced Materials Pearlbond® DIPP-119 Thermoplastic Polyurethane Pearlbond™ DIPP-119 is polycaprolactone copolyester based thermoplastic polyurethane, supplied in form of translucent pellets. Featuring low melting point and excellent transparency, this produ.. |
|||
Softening Point | 80.0 - 100 °C | 176 - 212 °F | |
Lucobit Lucobit® 1210A Ethylene Copolymer Bitumen Lucobit 1210A is a mixture of ethylene copolymers and special bitumen. Addition of Lucobit to bitumen increases its viscosity and broadens the range of plasticity.Lucobit 1210A in asphalt mixtures .. |
|||
Softening Point | 80.0 - 100 °C | 176 - 212 °F | |
Lucobit Lucolast® 7010 Ethylene Butyl Acrylate Asphalt Additive Lucolast® 7010 is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Addition of Lucolast 7010 to bitumen increases its viscosity, broadens the range of plasticit.. |
|||
Softening Point | 80.0 - 100 °C | 176 - 212 °F | flow beginning |
Taiwan Sheen Soon Sheenthane® AH-580 TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for soft hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes.. |
|||
Softening Point | 80.0 - 100 °C | 176 - 212 °F | flow beginning |
Taiwan Sheen Soon Sheenthane® AH-500 TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for soft hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes.. |
|||
Softening Point | 80.0 - 100 °C | 176 - 212 °F | flow beginning |
Taiwan Sheen Soon Sheenthane® AH-562 TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for soft hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes.. |
|||
Softening Point | 90.0 - 100 °C | 194 - 212 °F | |
DayGlo Gem-Tone GC-13P Ruby Red Gem-Tone® GC-13P Ruby Red is a rich, strong blue shade red colorant intended for use in clarified polypropylene. Clean, haze free, non-warping color formulations can easily be achieved with the use.. |
|||
Softening Point | 90.0 - 100 °C | 194 - 212 °F | |
Beijing Ranger Chem SM-604H Solid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Softening Point | 80.0 - 100 °C | 176 - 212 °F | flow beginning |
Taiwan Sheen Soon Sheenthane® AH-560T TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for soft hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes.. |