Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 388 °C | 730 °F | |
Ferro CF 8463 Low-Temperature Sealing VITREOUS Typical Powder Form: VSD, VWG Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific.. |