Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 124 °C | 255 °F | ETM 22-24 |
ExxonMobil ESCOREZ™ 5320 Petroleum Hydrocarbon Resin The Escorez 5300 series resins are water white cycloaliphatic hydrocarbon resins. They are designed to tackify a variety of adhesive polymers including EVA, SIS and SEBS block copolymers, APP an d A.. |
|||
Softening Point | 124 - 132 °C | 255 - 270 °F | |
Beijing Ranger Chem 197 Solid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |