Polymer Property : Softening Point = 205 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Softening Point 96.0 °C
205 °F
Zeon Chemicals Quintone® C200S Aliphatic Hydrocarbon Resin
C5 type (piperylene precursor). Has excellent flowability, heat stability and colors, suitable for traffic paint.Information provided by Zeon Chemicals L.P.
Softening Point 96.0 °C
205 °F
Zeon Chemicals Quintone® R100 Aliphatic Hydrocarbon Resin
C5 type (piperylene precursor). Gives well-balanced performance to adhesives; also suitable for hot melt adhesives.Information provided by Zeon Chemicals L.P.
Softening Point 96.0 - 107 °C
205 - 225 °F
Beijing Ranger Chem SM-604R Solid Epoxy Resin
Information provided by Beijing Ranger Chemical Co.