Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 710 °C | 1310 °F | Viscosity 10<sup>7.6</sup> dPa s; ISO 7884-3 |
Schott Glass 8625 Biocompatible Glass Biocompatible glass, high IR-absorbing, Transponders (implantable) The heavy metal content of the elements lead, cadmium, mercury, and hexavalent chromium is below 100 ppmInformation provided by S.. |
|||
Softening Point | 712 °C | 1310 °F | |
Schott S8807 Contrast Enhancement Filter Contrast Enhancement FilterInformation Provided by SCHOTT North America, Inc. |
|||
Softening Point | 712 °C | 1310 °F | |
Corning 7052 Alkali Barium Borosilicate Crushed/Powdered Glass Available in mesh sizes 4 through 325 and can be customized. Used for sealing and other applications.Information provided by Corning Incorporated. |