Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 60.0 - 70.0 °C | 140 - 158 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 115 Linear Thermoplastic Polyurethane
(discontinued **) PEARLBOND® 115 is a linear, aromatic polyurethane, supplied in form of white slightly yellowish pellets, which combines a very high crystallization rate with a high thermoplasticity level.Applicati.. |
|||
Softening Point | 50.0 - 70.0 °C | 122 - 158 °F | |
Hong Kun Group UV 622 UV Absorber Chemical Name: Poly (1-(2-hydroxyethyl)-2,2,6,6-tetramethyl-4-hydroxy-piperindinylsuccinate)CAS No. 65447-77-0All information provided by Hongkun Group |
|||
Softening Point | 65.0 - 70.0 °C | 149 - 158 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 104 Linear Thermoplastic Polyurethane Pearlbond™ 104.is a linear, aromatic polyurethane, supplied in form of small white or slightly yellowish granules, which combines a high crystallisation rate with a high thermoplasticity level... |
|||
Softening Point | 50.0 - 70.0 °C | 122 - 158 °F | |
Suqian Unitechem Light Stabilizer 622 Chemical Name: Poly-(N-Beta-hydroxyethyl-2,2,6,6-tetramethyl-4-hydroxy-piperidyl succinate)CAS NO.: 65447-77-0Molecular Formula: H[C15H25O4N]nOCH3Application: Hindered amine light stabilizer. It is.. |
|||
Softening Point | 50.0 - 70.0 °C | 122 - 158 °F | |
TSE Industries Millstab™ P Hydrolytic Stabilizer Additive Millstab P is a hydrolytic stabilizer for polyester polyurethane rubbers. The ester linkage of polyester urethanes is susceptible to attack by moisture, water, acids and bases. Millstab P will delay.. |
|||
Softening Point | 60.0 - 70.0 °C | 140 - 158 °F | |
Beijing Ranger Chem E-21 Solid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Softening Point | 50.0 - 70.0 °C | 122 - 158 °F | |
TSE Industries Millstab™ P Hydrolytic Stabilizer Additive Millstab P is a hydrolytic stabilizer for polyester polyurethane rubbers. The ester linkage of polyester urethanes is susceptible to attack by moisture, water, acids and bases. Millstab P will delay.. |
|||
Softening Point | 60.0 - 70.0 °C | 140 - 158 °F | Kofler; MQSA 70 A |
Lubrizol Advanced Materials Pearlbond® D183 Thermoplastic Polyurethane
(discontinued **) The Pearlbond® grades are aromatic crystalline TPUs used for the production of heat activated shoe counters and toe puffs, and orthopedic products. The Pearlbond® grades are supplied in pellet fo.. |