Thermal Properties Metric English Comments
Softening Point 124 - 132 °C
255 - 270 °F
Beijing Ranger Chem 197 Solid Epoxy Resin
Information provided by Beijing Ranger Chemical Co.
Softening Point 110 - 132 °C
230 - 270 °F
AdvanSource Biomaterials HydroMed™ D640 Permanently Lubricious Polyurethane Coating
AdvanSource Biomaterials Corporation manufactures and markets hydrophilic high slip, high water absorptive, polyether hydrophilic polyurethanes designed for use as coatings of catheters, sutures, in..
Softening Point 110 - 132 °C
230 - 270 °F
AdvanSource Biomaterials HydroSlip™ C Hydrophilic Polyether Aliphatic Polyurethane
AdvanSource Biomaterials Corporation manufactures and markets thermoplastic elastomeric hydrogels under the tradename HydroThane™. HydroThane™ is a generic family of polyurethane hydrogels, with ..