Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 96.0 °C | 205 °F | |
Zeon Chemicals Quintone® C200S Aliphatic Hydrocarbon Resin C5 type (piperylene precursor). Has excellent flowability, heat stability and colors, suitable for traffic paint.Information provided by Zeon Chemicals L.P. |
|||
Softening Point | 96.0 °C | 205 °F | |
Zeon Chemicals Quintone® R100 Aliphatic Hydrocarbon Resin C5 type (piperylene precursor). Gives well-balanced performance to adhesives; also suitable for hot melt adhesives.Information provided by Zeon Chemicals L.P. |
|||
Softening Point | 96.0 - 107 °C | 205 - 225 °F | |
Beijing Ranger Chem SM-604R Solid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |