Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 846 °C | 1550 °F | |
Potters Industries Spheriglass® 3000E Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |