Polymer Property : Softening Point = 77.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Softening Point 77.0 °C
171 °F
ISO 306
Iran Petrochemical (PCC) BL3 HF 4760 High Density Polyethylene
BL3 is a high density polyethylene with 1-Butene as co monomer. It is high density and stiffness, good ESCR, high rigidity, good flowability and impact strength.Applications: small blow molding, bo..
Softening Point 77.0 - 93.0 °C
171 - 199 °F
flow beginning
Taiwan Sheen Soon Sheenthane® AH-670 TPU for Hotmelt Adhesive
Thermoplastic polyurethane elastomer for hard hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes..
Softening Point 77.0 °C
171 °F
JIS K-2531
Unitika elitel UE3350 Polyester, Flake
Low molecular weight type UE3210, High OH typeUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesives, p..
Softening Point 77.0 - 80.0 °C
171 - 176 °F
DayGlo Gem-Tone GC-18F Emerald Green
Gem-Tone® GC-18F Emerald Green is a rich, strong green colorant intended for use in clarified polypropylene. Clean, haze free, non-warping color formulations can easily be achieved with the use of ..
Softening Point 77.0 - 81.0 °C
171 - 178 °F
Beijing Ranger Chem WSR601 Solid Epoxy Resin
Information provided by Beijing Ranger Chemical Co.
Softening Point 77.0 - 81.0 °C
171 - 178 °F
Beijing Ranger Chem WSR603 Solid Epoxy Resin
Information provided by Beijing Ranger Chemical Co.