Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 715 °C | 1320 °F | Viscosity 10<sup>7.6</sup> dPa s; ISO 7884-3 |
Schott Glass 8242 Borosilicate Glass Borosilicate glass for sealing to Kovar metal and molybdenum, electrically highly insulating, low refractive index Clad tube for optical fibers, glass metal sealing The heavy metal content for the.. |
|||
Softening Point | 715 °C | 1320 °F | Viscosity 10<sup>7.6</sup> dPa s; ISO 7884-3 |
Schott Glass 8271 Borosilicate Glass Borosilicate glass, highly UV-blocked, stabilized against solarization. Used for sealing glass to KOVAR metal and backlights. The heavy metal content for the elements lead, cadmium, mercury, and hex.. |