Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 712 °C | 1310 °F | |
Schott S8807 Contrast Enhancement Filter Contrast Enhancement FilterInformation Provided by SCHOTT North America, Inc. |
|||
Softening Point | 712 °C | 1310 °F | |
Corning 7052 Alkali Barium Borosilicate Crushed/Powdered Glass Available in mesh sizes 4 through 325 and can be customized. Used for sealing and other applications.Information provided by Corning Incorporated. |