Softening Point 585 °C
1090 °F
Viscosity 10<sup>7.6</sup> dPa s; ISO 7884-3
Schott Glass 8531 Soft Glass
Soft glass, free from Na, of high lead content, high dielectric constant Encapsulation of semiconductor components at low temperature (diodes)Information provided by SCHOTT AG.