Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 125 °C | 257 °F | T5 Point; modulus = 690 MPa (100,000 psi) |
Specialty Coating Systems Parylene C Poly (P-Xylylene) Coating Parylene C is a polymer of para-xylylene modified by the substitution of a chlorine atom for one of the aromatic hydrogen atoms. Parylene C has a useful combination of electrical and physical proper.. |
|||
Softening Point | 125 °C | 257 °F | T5 Point; modulus = 690 MPa (100,000 psi) |
Specialty Coating Systems Parylene D Poly (P-Xylylene) Coating Parylene D is a polymer of para-xylylene modified by the substitution of chlorine atoms for two of the aromatic hydrogen atoms. Parylene D is similar in properties to Parylene C with the added abili.. |