Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 115 °C | 239 °F | JIS K-2531 |
Unitika elitel UE3230 Polyester, Flake Adhesive agent, Resin modifierUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesives, paints, ink binde.. |
|||
Softening Point | 115 °C | 239 °F | Flow beginning temperature |
Wanhua Chemical Wanthane® WHT-6226 TPU Hot-Melt Adhesive Wide range of activation temperature, fast crystallization rate, outstanding bonding strength for fabrics, leathers, plastics & rubbers, wood, etc.Information provided by Wanhua Chemical Group Co., .. |
|||
Softening Point | 115 °C | 239 °F | |
Zeon Chemicals Quintone® G115 Aliphatic Hydrocarbon Resin C5/C9 type (piperylene and dicyclopentadiene precursor).Information provided by Zeon Chemicals L.P. |
|||
Softening Point | 115 - 135 °C | 239 - 275 °F | |
Beijing Ranger Chem SM-607 Solid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Softening Point | 115 °C | 239 °F | Flow beginning temperature |
Wanhua Chemical Wanthane® WHT-6233 TPU Hot-Melt Adhesive Wide range of activation temperature, fast crystallization rate, outstanding bonding strength for fabrics, leathers, plastics & rubbers, wood, etc.Information provided by Wanhua Chemical Group Co., .. |
|||
Softening Point | 115 - 120 °C | 239 - 248 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 151 Linear Thermoplastic Polyurethane
(discontinued **) PEARLBOND® 125/H is polycaprolactone-based thermoplastic polyurethane, supplied in form of colourless or slightly yellowish, translucid pellets, combining a low hardness with excellent low-temperat.. |
|||
Softening Point | 115 °C | 239 °F | Flow beginning temperature |
Wanhua Chemical Wanthane® WHT-6232 TPU Hot-Melt Adhesive Wide range of activation temperature, fast crystallization rate, outstanding bonding strength for fabrics, leathers, plastics & rubbers, wood, etc.Information provided by Wanhua Chemical Group Co., .. |