Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 123 - 290 °C
254 - 554 °F
Average value: 276 °C Grade Count:18
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an..
Deflection Temperature at 1.8 MPa (264 psi) 274 - 290 °C
525 - 554 °F
Average value: 284 °C Grade Count:10
Overview of materials for Nylon 46, Lubricated + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Lubricated + Glass Fiber Reinforced". Each property range of values reported is minimum and ma..