Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 40.6 - 222 °C
105 - 432 °F
Average value: 95.5 °C Grade Count:109
Overview of materials for Polycarbonate/PET Polyester Blend
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values..
Deflection Temperature at 1.8 MPa (264 psi) 180 - 222 °C
356 - 432 °F
Average value: 193 °C Grade Count:8
Overview of materials for Phenolic, Novolac, Mineral/Graphite Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Graphite Filled". Each property range of values reported is minimum and maxim..