Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-07 |
Proto3000 Objet FullCure720 Transparent Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-07 |
Proto3000 Objet VeroBlack FullCure870 Rigid Opaque Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-07 |
Proto3000 Objet VeroBlue FullCure840 Rigid Opaque Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-07 |
Proto3000 Objet VeroClear FullCure810 Information provided by Proto3000 for their protoyping engineering services. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-07 |
Proto3000 Objet VeroGray FullCure850 Rigid Opaque Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 48.0 - 50.0 °C | 118 - 122 °F | ASTM D648-98c |
DSM Somos® ProtoGen™ O-XT 18120 Epoxy Resin for Stereolithography, UV Postcure at HOC -2 DescriptionDSM Somos® ProtoGen O-XT 18120 is a liquid photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demonstrate diffe.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 49.0 - 50.0 °C | 120 - 122 °F | Thermal Postcure; ASTM D648-98c |
DSM Somos® WaterClear® Ultra 10122 Optically Clear, Colorless, Rigid, Stereolithography Resin DescriptionDSM Somos® WaterClear Ultra 10122 is a next generation optically clear resin with ABS like properties and good temperature resistance. It produces colorless, functional, accurate parts .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 48.0 - 50.0 °C | 118 - 122 °F | ASTM D648 |
3D Systems Accura® 60 Plastic for SLA® Systems Simulate the properties and appearance of polycarbonate. For use with solid-state stereolithography (SLA®) systems.ApplicationsTough functional prototypesAutomotive design componentsConsumer electr.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 48.0 - 50.0 °C | 118 - 122 °F | ASTM D648 |
Proto3000 Accura® 60 Plastic Stereolithography (SLA) Prototyping Polymer Features:Durable and stiffHigh clarityFast build speedLow viscosity formulationHumidity resistant partsFully developed and tested build stylesBenefits:Achieve the look and feel of polycarbonateView .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-07 |
Proto3000 Objet VeroWhitePlus FullCure835 Rigid Opaque Prototyping Polymer Information provided by Proto3000 for their protoyping engineering services. |