Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 301 °C | 574 °F | ASTM D648 |
Solvay Specialty Polymers Amodel® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry as Molded
(d AMODEL FR-4133 is a 33% glass-reinforced polyphthalamide (PPA) resin designed for electrical and electronic applications. This UL94-V0 resin offers the highest mechanical and electrical properties, .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 301 °C | 574 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PPA GF30 HS L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Temperature StrengthInformat.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 301 °C | 574 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® TPX-HTN-01027 A 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Temperature StrengthUL File .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 301 °C | 574 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® HTN 01400 BK Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, High Heat Resistance and LubricatedAppearance: BlackInformation provided by TP Composites, .. |