Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 288 °C | 550 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA4/6 GF45 HS BK 45% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 45% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackTPCI# 9627150Informat.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 288 °C | 550 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PEEK CF20 TL15 HF 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: High Flow and LubricatedInformation provided by TP Composi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 288 °C | 550 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PEEK CF30 HF 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 30% Filler by WeightFeatures: High FlowInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 288 °C | 550 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® TPX-HTN-02028 A 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Temperature StrengthInformat.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 288 °C | 550 °F | ASTM D648 |
Resinoid 1322 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 288 °C | 550 °F | Unannealed; ISO 75-2/A |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA)
(Unverified Data**) Amodel A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high strength.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 288 °C | 550 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA4/6 GF30 FR HS L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, Flame Retardant and Lu.. |