Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 236 °C
457 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics Extem UH1016M TPI Blend
High heat amorphous TPI Blend, Chemical ResistantThis data was supplied by SABIC-IP for the Americas region.
Deflection Temperature at 1.8 MPa (264 psi) 236 °C
457 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics Extem UH1016M TPI Blend (Asia Pacific)
High heat amorphous TPI Blend, Chemical ResistantThis data was supplied by SABIC-IP for the Asia Pacific region.
Deflection Temperature at 1.8 MPa (264 psi) 236 °C
457 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics Extem UH1016M TPI Blend (Europe-Africa-Middle East)
High heat amorphous TPI Blend, Chemical ResistantThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Deflection Temperature at 1.8 MPa (264 psi) 236 °C
457 °F
Annealed; ISO 75-2/A
PolyOne Bergamid™ A70 G35 H U BK SO Polyamide 66 (Nylon 66)
Information provided by PolyOne
Deflection Temperature at 1.8 MPa (264 psi) 236 °C
457 °F
Unannealed; ISO 75-2/A
PolyOne Bergamid™ A70 G35 UF SO Polyamide 66 (Nylon 66)
Information provided by PolyOne
Deflection Temperature at 1.8 MPa (264 psi) 236 °C
457 °F
ISO 75-1,-2
Gromax CFG45-PN11N1 Nylon 6 46% Glass Filled (Conditioned)
Information provided by Gromax Enterprises Corp.
Deflection Temperature at 1.8 MPa (264 psi) 236 °C
457 °F
ISO 75-1,-2
Gromax CFG45-PN11N1 Nylon 6 46% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Deflection Temperature at 1.8 MPa (264 psi) 236 °C
457 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP LUBRICOMP RFI12 PA 66
LNP* LUBRICOMP* RFI12 is a compound based on Nylon 66 resin containing 10% Glass Fiber, 2% Silicone. Added feature of this material is: Wear Resistant.
Deflection Temperature at 1.8 MPa (264 psi) 236 °C
457 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP LUBRICOMP RFL22E PA6.6 (Europe-Africa-Middle East)
LNP* LUBRICOMP* RFL22E Is a compound based on PA66 resin, containing Glass Fiber and PTFE. Added features include: Internally Lubricated, Easy Moulding
Deflection Temperature at 1.8 MPa (264 psi) 236 °C

@Thickness 3.20 mm
457 °F

@Thickness 0.126 in
unannealed; ASTM D 648
SABIC Innovative Plastics LNP Lubricomp RFM62 PA 66
LNP* Lubricomp* RFM62 is a compound based on Nylon 66 resin containing Glass Fiber, Mineral.This data was supplied by SABIC-IP for the Americas region.
Deflection Temperature at 1.8 MPa (264 psi) 236 °C

@Thickness 3.20 mm
457 °F

@Thickness 0.126 in
unannealed; ASTM D 648
SABIC Innovative Plastics LNP Lubricomp RFM62 PA 66 (Asia Pacific)
LNP* Lubricomp* RFM62 is a compound based on Nylon 66 resin containing Glass Fiber, Mineral.This data was supplied by SABIC-IP for the Asia Pacific region.
Deflection Temperature at 1.8 MPa (264 psi) 236 °C
457 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP LUBRICOMP RFP36 PA 66
LNP* LUBRICOMP* RFP36 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% PTFE, Silicone. Added features of this material include: Wear Resistant.
Deflection Temperature at 1.8 MPa (264 psi) 236 °C
457 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP LUBRICOMP RFP36 PA 66 (Asia Pacific)
LNP* Lubricomp* RFP36 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE, Silicone. Added features of this material include: Internally Lubricated. This product is also known as Lub..
Deflection Temperature at 1.8 MPa (264 psi) 236 °C
457 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP LUBRICOMP RFP36 PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RFP36 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE, Silicone.
Deflection Temperature at 1.8 MPa (264 psi) 236 °C
457 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP LUBRICOMP RFP36S PA 66
LNP* LUBRICOMP* RFP36S is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Wear Resistant, Heat Stabilized.
Deflection Temperature at 1.8 MPa (264 psi) 236 °C
457 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP LUBRICOMP RFP36XXZ PA 66 (Asia Pacific)
LNP Lubricomp RFP36XXZ is a compound based on Nylon 66 resin containing Glass Fiber, PTFE, Silicone. Added features of this material include: internally lubricated. Also known as Lubricomp RFL-4536 ..
Deflection Temperature at 1.8 MPa (264 psi) 236 °C

@Thickness 3.20 mm
457 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP STAT-KON RFD02 PA 66
LNP* STAT-KON* RFD02 is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Electrically Conductive.
Deflection Temperature at 1.8 MPa (264 psi) 236 °C

@Thickness 3.20 mm
457 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP STAT-KON RFD02 PA 66 (Asia Pacific)
LNP* Stat-kon* RFD02 is a compound based on Nylon 66 resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive.
Deflection Temperature at 1.8 MPa (264 psi) 236 °C

@Thickness 3.20 mm
457 °F

@Thickness 0.126 in
unannealed; ASTM D 648
SABIC Innovative Plastics LNP Thermocomp RF004S PA 66
LNP* Thermocomp* RF004S is a Nylon 6/6 containing Glass Fiber. Characteristics are Heat Stabilized.This data was supplied by SABIC-IP for the Americas region.
Deflection Temperature at 1.8 MPa (264 psi) 236 °C
457 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP THERMOCOMP RF006 PA 66
LNP* THERMOCOMP* RF006 is a compound based on Nylon 66 resin containing 30% Glass Fiber.
Deflection Temperature at 1.8 MPa (264 psi) 236 °C
457 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP THERMOCOMP RF006S PA 66
LNP* THERMOCOMP* RF006S is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized.
Deflection Temperature at 1.8 MPa (264 psi) 236 °C
457 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP THERMOCOMP RF006XXH PA 66
LNP* THERMOCOMP* RF006XXH is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added feature of this material is: Healthcare.
Deflection Temperature at 1.8 MPa (264 psi) 236 °C

@Thickness 3.20 mm
457 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP RX08401 PA 66
LNP* Thermocomp* RX08401 is a compound based on Nylon 66 containing Glass Fiber. Added feature of this grade include: Impact Modified.
Deflection Temperature at 1.8 MPa (264 psi) 236 °C
457 °F
Flatw 80x10x4, sp=64 mm; ISO 75/Af
Eurostar Star L PA66 30V D31 PA66, Glass Fiber Filled, Injection Molded
Star L PA66 30V D31 is a Molybdenum Disulfide Lubricated, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Deflection Temperature at 1.8 MPa (264 psi) 236 °C
457 °F
ASTM D648
Ashley Polymers Ashlene® 520S-13GU Nylon 66, 13% Glass Reinforced
Nylon 66, 13% Glass reinforced resin with heat stabilizer, utility grade. Also available in black (520S-13GBU).Data provided by the manufacturer
Deflection Temperature at 1.8 MPa (264 psi) 236 °C
457 °F
ASTM D648
A. Schulman ComAlloy Voloy® 688 Nylon 6/6, Glass Fiber/Bead Reinforced, Nylon 6/6 Alloy, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.45% Glass Fiber/Bead Reinforced. Halogen- and phosphorous-freeThe ComAlloy product line has been integrated into the A Schulman prod..