Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 234 °C | 453 °F | ASTM D648 |
Nylene® PA6/6 Glass/Mineral Filled 7215 HS Nylon 6/6 15% Glass Reinforced/25% Mineral Filled.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 234 °C @Thickness 3.20 mm |
453 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics EXTEM UH1026 TPI Blend High heat amorphous TPI Blend, Chemical Resistant, High Flow, IR-Transparent |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 234 °C | 453 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® HTN 53G50HSLR BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN53G50HSLR BK083 is a 50% glass reinforced, heat stabilized, lubricated high performance polyamide resin developed for moderate temperature structural applications requiring retention of h.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 234 °C | 453 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP STAT-KON OEL32 PPS - Linear LNP* STAT-KON* OCL32 is a compound based on PPS - Linear resin containing 10% Carbon Fiber, 15% PTFE. Added features of this grade include: Electrically Conductive, Wear Resistant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 234 °C | 453 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP STAT-KON REP349 PA 66 LNP* STAT-KON* REP349 is a compound based on Nylon 66 resin containing 15% PTFE/Silicone, 20% Carbon Fiber. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 234 °C | 453 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP STAT-KON REP349 PA 66 (Asia Pacific) LNP* Stat-kon* REP349 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 234 °C | 453 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Thermocomp RF006PS PA 66 LNP* Thermocomp* RF-1006 EP HS is based on Nylon 6/6 containing Glass Fiber. Characteristics of this grade include Exceptional Processing and Heat Stabilizer.This data was supplied by SABIC-IP for .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 234 °C | 453 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP RFB53XXZ PA 66 LNP* THERMOCOMP* RFB53XXZ is a compound based on Nylon 66 resin containing 15% Glass Fiber, 25% Glass Bead. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 234 °C | 453 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Thermocomp RX06423 PA 66 LNP* Thermocomp* RX06423 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized.This data was supplied b.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 234 °C | 453 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP RX99732C PA 66 LNP* Thermocomp* PDX-R-99732 is a Nylon 6/6 with proprietary fillers. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 234 °C @Thickness 3.20 mm |
453 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP RX99732C PA 66 LNP* Thermocomp* PDX-R-99732 is a Nylon 6/6 with proprietary fillers. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 234 °C @Thickness 3.20 mm |
453 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Noryl GTX APS8740 PPE+PPS Noryl* APS8740 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can be e.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 234 °C @Thickness 3.20 mm |
453 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Noryl GTX APS8740 PPE+PPS (Asia Pacific) Noryl* APS8740 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can be e.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 234 °C @Thickness 3.20 mm |
453 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Noryl GTX APS8740 PPE+PPS (Europe-Africa-Middle East) Noryl* APS8740 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can be e.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 234 °C @Thickness 3.20 mm |
453 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL GTX EXNX0080 PPE+PPS Noryl APS* EXNX0080 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 234 °C @Thickness 3.20 mm |
453 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL GTX EXNX0080 PPE+PPS (Asia Pacific) Noryl APS* EXNX0080 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 234 °C @Thickness 3.20 mm |
453 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL GTX EXNX0080 PPE+PPS (Europe-Africa-Middle East) Noryl APS* EXNX0080 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 234 °C | 453 °F | ISO 75-1, 2 |
Polyplastics FR-PET® B9030 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose Information provided by PolyPlastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 234 °C | 453 °F | ISO 75-1, 2 |
Polyplastics FR-PET® C9030 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose Information provided by PolyPlastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 234 °C | 453 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® HTN 53G50HSLR BK083 Polyphthalamide (PPA)
(Unverified Data**) 50% Glass Reinforced High Performance Polyamide with Improved Impact and Stiffness Zytel HTN53G50HSLR BK083 is a 50% glass reinforced heat stabilized lubricated high performance polyamide resin deve.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 234 °C | 453 °F | ASTM D648 |
A. Schulman ComAlloy Hiloy® 657 Nylon 6/6, Carbon/Glass Fiber Reinforced, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |