Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | |
Plastcom SLOVAMID 6 NG GF 45 SGF PA6, improved strength, light stability FeaturesPA 6 for injection moulding, chemically strengthened with 45 % of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-goo.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | ISO 75 |
Nilit FRIANYL B63 KF20 Nylon 6 for injection molding, 20% short glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | ASTM D648 |
Quadrant EPP Semitron® MDS 100 (ASTM Product Data Sheet) |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | ISO 75-1/-2 |
Lanxess Pocan® T 7391 POS151 000000 PBT + PET, 45% Glass Fiber
(discontinued **) PBT+PET, 45% glass fibers, injection molding, improved surface finish, increased temperature peak load, UV-stabilized |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | ASTM D648 |
Quadrant EPP Duratron® PEI U2300 Extruded 30% Glass Reinforced Polyetherimide (ASTM Product Data Sheet) |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | Unannealed; ASTM D648 |
LNP Lubricomp® EFL-4544 Polyetherimide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | ISO 75-1/-2 |
Lanxess Pocan® BF 4235 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 210 °C @Thickness 3.20 mm |
410 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP WFL34 PBT LNP LUBRICOMP* WFL34 is a compound based on PBT resin containing 20% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 210 °C @Thickness 6.40 mm |
410 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Valox® IQNH4560 PBT (Asia Pacific) Valox* IQNH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* iQ PBT resin. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | |
Shinil Chemical SHINCON PEI-CNT LCD Rack LCD Rack is used to transfer or bake LCD frame in the electronic assembly or LCD packaging assembly line. Current LCD Rack is made of poly ether ether ketone (PEEK) with carbon fiber (CF). Since b.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | ASTM D648 |
Samyang Tribit® 1550GN30 PBT Alloy, Reinforced Flame Retardancy Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1550GN30 is a reinforced, flame retardant (.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 210 °C @Thickness 3.20 mm |
410 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP WCL36 PBT LNP* LUBRICOMP* WCL36 is a compound based on PBT resin containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include: Electrically Conductive, Wear Resistant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | ISO 75-1, 2 |
Polyplastics Duranex® 7390W Polybutylene Terephthalate (PBT), Super low warpage, GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | ASTM D648 |
A. Schulman ComAlloy® E-12421 Reinforced High Flow Polyamide Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | ISO 75-1, 2 |
Polyplastics Duranex® 3300H Polybutylene Terephthalate (PBT), Standard, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | ISO 75-1/-2 |
DSM Arnite® TV4 260 SXF PBT-GF30 FR(17) 30% Glass Reinforced, Flame Retardant, High Flow |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | 1/4''; ASTM D648 |
Ensinger TECAPEI® 30% Glass Reinforced, made from Ultem® 2300 PEI TECAPEI™ is an amorphous thermoplastic polyetherimide (PEI) made from Sabic Innovative Plastics' Ultem® 1000 and 2000 series resins. The unreinforced 1000 series materials are translucent amber in.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | ASTM D648 |
Clariant PA612G30 Nylon 612, 30% Glass Fiber, Impact Modified Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | ISO 75 |
Eurotec® Tecopet® PT70 GR30 NL100 MB PET, 30% glass fiber reinforced, impact modified, heat stabilized, natural Information provided by Eurotec® |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | ISO 75-1/-2 |
DSM Akulon® K224-G6 (Dry) 30% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | ISO 75 |
Azoty Tarnow™ Tarnamid® T-27 GF30 Polyamide 6 - Glass Fiber Reinforced 30% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | ISO 75 |
Azoty Tarnow™ Tarnamid® T-27 GF35 Polyamide 6 - Glass Fiber Reinforced 35% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | ASTM D648 |
Asahi Kasei Thermylon® NSG-240A-C 50% Ceramic and Glass Fiber Reinforced Information provided by Asahi Thermofil |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | ASTM D648 |
Ashley Polymers Ashlene® 827L-25G Nylon 6, 25% Glass Reinforced A 25% glass reinforced high impact Nylon 6 designed for applications requiring a high level of toughness, as well as superior low temperature properties.Data provided by the manufacturer |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | ISO 75-2 |
BASF Ultradur® FRee B 4440 G5 25% Glass Filled PBT Description: Is a PBT, injection-molding grade with 25% glass fibers for parts requiring enhanced fire resistance as well as increased tracking resistance (e.g. housings for electronics, plug-and-so.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | ASTM Data |
BASF Capron® 8332G Impact Modified, 25% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8332G is a 25% glass reinforced, impact modified polyamide 6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a balance of .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | ISO 75-1/-2 |
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness and sur.. |