Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 335.0 °F
Polymer Property :
Deflection Temperature at 1.8 MPa (264 psi) =
335.0 °F
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
168.3
°C
335.0
°F
ASTM D648
PTS PBT-15GF 15% Glass Filled PBT