Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 129 °C | 265 °F | ASTM D648 |
Polymer Resources PC-FR2-TFE Polycarbonate, Flame Retardant, 5% PTFE Polycarbonate, Improved Flame Retardant, 5% PTFE LubricantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 129 °C | 265 °F | ASTM D648 |
Polymer Resources PC-FR3-D-[color]-3 Polycarbonate, Improved Flame Retardant, High Flow, UV-stabilized Polycarbonate, Improved Flame Retardant, High Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 129 °C | 265 °F | ASTM D648 |
Polymer Resources PC-GP2-D Polycarbonate, General Purpose, Medium Flow Polycarbonate, General Purpose, Medium FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 129 °C | 265 °F | ASTM D648 |
Polymer Resources PC-UV2-D-[color]-1 Polycarbonate, UV-stabilized, Medium Flow with Mold Release Polycarbonate, UV-stabilized, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 129 °C | 265 °F | ASTM D648 |
Polymer Resources PPX-FRG30 Modified-PPO, V-1 Flame Retardant, 30% Glass Reinforced Modified-Polyphenylene Oxide, V-1 Flame Retardant, 30% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 129 °C | 265 °F | ASTM D648 |
Nylene® Naxel™ PC35CV Polycarbonate Description: Naxel™ PC35CV is a 12 melt, virgin, general purpose polycarbonate. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 129 °C | 265 °F | ASTM D648 |
Polymer Resources PPX-FRG30 Modified PPO, UL 94 V-1, 30% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 129 °C | 265 °F | ASTM D648 |
Polymer Resources PC-FD2 Polycarbonate, FDA-compliant Feedstocks, Medium Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Medium Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 129 °C | 265 °F | ASTM D648 |
Polymer Resources PC-FR1-D-[color]-3 Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilized Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 129 °C | 265 °F | Unannealed (0.250"); ASTM D648 |
LTL Color Compounds ColorFast® PC150 Polycarbonate 15 melt high flow polycarbonateAll information provided by LTL Color Compounders, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 129 °C | 265 °F | ASTM D648 |
Fiberfil® J-68/10/E Polypropylene Copolymer, 10% Glass Fiber Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 129 °C | 265 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® PC 04007 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackTPCI# 9691124Information provided by.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 129 °C | 265 °F | unannealed, .125in; ASTM D648 |
Star Plastics PC733R Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 129 °C | 265 °F | unannealed, .125in; ASTM D648 |
Star Plastics PC741 Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 129 °C | 265 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP GF10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 129 °C | 265 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® PC TL15 Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 129 °C | 265 °F | Unannealed, 0.125 in; ASTM D648 |
Styron CALIBREâ„¢ 201-06 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 129 °C | 265 °F | Unannealed, 0.125 in; ASTM D648 |
Styron CALIBREâ„¢ 301-06 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 129 °C | 265 °F | 0.157 in, unannealed; ASTM D648 |
Styron EMERGEâ„¢ 4330-6 Polycarbonate EMERGEâ„¢ PC 4330-6 advanced resin is a polycarbonate resin offering ultraviolet light stability, high heat resistance and maximum toughness. Applications: Consumer Electronics and Information .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 129 °C | 265 °F | ASTM D648 |
Chase Plastics CP Pryme® PC100RUV Polycarbonate, Mold Release, UV Stabilized Information provided by Chase Plastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 129 °C | 265 °F | Unannealed; ASTM D648 |
Entec Hylex® P1317FR Polycarbonate Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 129 °C | 265 °F | ASTM D648 |
Entec Hylex® P1317L1 HB Polycarbonate UV Stabilized, Higher Flow, Mold Release, Water ClearInformation provided by Entec. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 129 °C | 265 °F | ASTM D648 |
Polymer Resources PPX/NY GP2 Modified PPO, Medium Heat PPX/Nylon 6,6 Alloy
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 129 °C | 265 °F | ASTM D648 |
RheTech Products G20P252-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Natural Applications: Interior trimArm rest insertConsolesDome light housingInjection molding conditions reported in table.Information provided by RheTech Products. |