Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 120.5 °C | 248.9 °F | unannealed; ASTM D648 |
KYDEX® FST Fully Compliant Aviation Thermoforming Sheet KYDEX® FST meets all fire, smoke and heat release requirements set forth by the Federal Aviation Regulations 25.853 paragraphs (a) and (d) as well as toxicity requirements for ABD0031, BSS7239 an.. |