Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 101 °C | 213 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hysun™ A3525 ASA+PC Available in North America Features: Good Impact Resistance RoHS CompliantForm: PelletsInformation provided by Ravago |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 101 °C | 213 °F | ASTM D648 |
Polymer Resources ABS-G20 ABS, 20% Glass Reinforced Acrylonitrile Butadiene Styrene, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |