Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 98.3 °C @Thickness 6.35 mm |
209 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne Edgetek® XT XT-100-BU01-HF Polycarbonate + PBT (PC+PBT) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.3 °C | 209 °F | ASTM D648 |
Polymer Resources ABS-G15 ABS, 15% Glass Reinforced Acrylonitrile Butadiene Styrene, 15% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.3 °C | 209 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers ASA/PC TA-35 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.3 °C @Thickness 6.35 mm |
209 °F @Thickness 0.250 in |
Annealed; ASTM D648 |
PolyOne Edgetek® XT XT-100-CX00 PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.3 °C @Thickness 6.35 mm |
209 °F @Thickness 0.250 in |
Annealed; ASTM D648 |
PolyOne Edgetek® XT XT-100-CX02-EG PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |