Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 76.6 °C | 170 °F | Annealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion LR620 white 1046 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | Unannealed; ASTM D648 |
Oxford Polymers C-Acetal -30GF-Natural Acetal Copolymer, 30% Glass Fiber Reinforced Product Description: Glass Fiber (30% Reinforced), Co-polymer Acetal, Injection Molding Grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Glass FiberSpecial Characteristic.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | ASTM D648 |
Polymer Resources PPX-FR4 Modified-PPO, V-1 Flame Retardant Modified-Polyphenylene Oxide, V-1 Flame Retardant, 185F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | unannealed; injection molded; ASTM D648 |
Americas Styrenics STYRON™ A-TECH™ 1220 High-Impact Polystyrene Resin
(discontinued **) STYRON™ A-TECH™ 1220 advanced technology polystyrene resin is a high impact, high modulus resin for extrusion thermoforming applications. The improved durability of this resin allows potential do.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C @Thickness 3.17 mm |
170 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
M. Holland Company AB308LG ABS Acrylonitrile Butadiene Styrene High flowGood impact resistanceHigh stiffnessApplications: Household goodsPackagingInformation provided by M. Holland |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | ASTM D648 |
Fiberfil® PP-60/V2 Polypropylene Homopolymer, Flame Retardant, UL94 V2 Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | ASTM D648 |
Fiberfil® PP-68/TC/20 Polypropylene Copolymer, 20% Talc Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | Unannealed (0.250"); ASTM D648 |
LTL Color Compounds ColorFast® FRA203 ABS Business machinery V0 ABS with excellent indoor light stabilityAll information provided by LTL Color Compounders, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | ASTM D648 |
Spartech Royalite R59 ABS/PVC Fire Rated Sheet Description: Fire Rated SheetInformation provided by Spartech. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 L N MB (Dry) Availability: North AmericaForms: PelletsAdditive: Lubricant and Nucleating AgentFeatures: Lubricated, Fast Molding Cycle, Good Processability and NucleatedTPCI# 7964102Information provided by TP Co.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 L N YL038MB Availability: North AmericaForms: PelletsAdditive: Lubricant, UV Stabilizer and Nucleating AgentFeatures: Lubricated, Fast Molding Cycle, Good Processability, Good UV Resistance and NucleatedAppeara.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | unannealed, .125in; ASTM D648 |
Star Plastics ABS5035 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® PA6/6,6 L N Nylon 6/66 Availability: North AmericaForms: PelletsAdditive: Nucleating Agent and LubricantFeatures: Copolymer, Fast Molding Cycle, Nucleated and LubricatedProcessing Method: Injection MoldingInformation prov.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® PC/ABS FR 2810 Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | Unannealed; 103°C (217°F) annealed; ASTM Data |
Styron Magnum™ 9700HF ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1512E Talc Filled, High Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1512E is a 10% talc-filled, high impact copolymer polypropylene. ApplicationPolyfort® FPP 1512E is suitable for extrusion or blow molding applications. Information provid.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1512E Talc Filled, High Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1512E is a 10% talc-filled, high impact copolymer polypropylene. ApplicationPolyfort® FPP 1512E is suitable for extrusion or blow molding applications. Information provid.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | Annealed; ASTM Data |
Dow Retain® PS-4578 Polystyrene Data provided by Dow Chemical. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | ASTM D648 |
Clariant 612-01 HSL Black Nylon 612, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | ASTM D648 |
Clariant Renol 612-01L Nylon 612, Lubricated Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | ASTM D648 |
Clariant Renol SB83642580 ASA Polymer Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | Unannealed; ASTM D648 |
LNP Lubricomp® IBL-4416 Polyamide 6/12 Copolymer, Glass Bead Reinforced, Silicone Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | ASTM D648 |
RheTech Products HP510-01UV 28% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black Applications: Air ducts-structuralInterior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 - 202 °C | 170 - 395 °F | Average value: 139 °C Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Aramid Fiber Filled". Each property range of values reported is minimu.. |