Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 70.6 °C | 159 °F | ASTM D648 |
Niche Polymer PPCT40BK Copolymer PP, 40% Talc Filled Information provided by Niche Polymer |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 70.6 °C @Thickness 3.18 mm |
159 °F @Thickness 0.125 in |
Annealed; ASTM D648 |
PolyOne Geon™ Vinyl Fittings M1015 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 70.6 °C | 159 °F | ASTM D648 |
Americas Styrenics STYRON A-TECH® 1260 High Impact Polystyrene Product CharacteristicsGood Environmental Stress Crack Resistance (ESCR)Good practical toughnessDeep draw thermoforming capableGood low temperature impactFood Contact CompliantTypical ApplicationsPa.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 70.6 °C | 159 °F | |
BCC Products BC 5008-2 General Purpose Epoxy System BC 5008-2 is a very low viscosity, modified, unfilled, room temperature curing, general purpose resin system. BC 5008-2 is a clear, amber, medium pot life material, with heat resistance to 175ºF. A.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 70.6 °C | 159 °F | annealed; ASTM D-648 |
Axiall 6511 Rigid PVC, Molding Georgia Gulf 6511 is a special purpose rigid PVC compound designed for applications requiring the following properties: GlossImpact Strength & ToughnessFlame RetardantChemical ResistantThermoformab.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 70.5 °C | 159 °F | annealed; ASTM D648 |
Kleerdex Kydex® 510 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Weatherable and decorative sheetApplications: Housings for equipment, recreation vehicles and truck parts, safety equipment, building products, signage, wall panels, facia, doors, service counters, .. |