Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 52.8 °C | 127 °F | ASTM D648 |
RheTech Products P256-762 Polypropylene Copolymer, Medium Grey Applications: Misc. ClipsElectrical housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.8 °C | 127 °F | ASTM D648 |
Nylene® 8100 Unfilled Nylon 6/12 Description: Nylene® 8100 is an unfilled specialty fiber. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.0 °C | 127 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYfill PPC T1010 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.0 °C | 127 °F | ASTM D648 |
North Wood Plastics HDPE with 40% Wood Fiber Data provided by North Wood Plastics, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.8 °C | 127 °F | ASTM D648 |
Polymer Resources TP-GP1F Polybutylene Terephthalate, General Purpose, FDA-compliant Feedstocks Polybutylene Terephthalate, General Purpose, FDA-compliant FeedstocksProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.8 °C | 127 °F | ASTM D648 |
Polymer Resources TP-GP1-IM Polybutylene Terephthalate, Impact Modified, Medium Flow Polybutylene Terephthalate, Impact Modified, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.0 °C | 127 °F | ASTM D648 |
PTS PBT-101G0 PBT Resin Typical Applications: Appliance partsInformation provided by PTS LLC. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.0 °C | 127 °F | ISO 75-1, -2 |
Lanxess Durethan® BC 550 Z DUSXBL 900116 Nylon 6, Impact Modified PA 6, non-reinforced, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.0 °C | 127 °F | ISO 75-1, -2 |
Lanxess Durethan® TP 142-011 900116 Nylon 6 PA 6, non-reinforced, extrusion, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.0 °C @Thickness 3.20 mm |
127 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP FL004 PE LNP* Lubricomp* FL004 is a compound based on Polyethylene resin containing 20% PTFE. Added features of this material include: Internally Lubricated. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.0 °C @Thickness 3.20 mm |
127 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics LNP Lubricomp PL004 PA 6 LNP* Lubricomp* PL004 is a compound based on Nylon 6 containing PTFE Lubricant. Characteristics of this grade are Internally Lubricated.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.0 °C @Thickness 3.20 mm |
127 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-KON MX10301C PP LNP* STAT-KON* MX10301C is a compound based on Polypropylene containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Clean Compounding System. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.0 °C | 127 °F | ISO 75-2 |
Borealis HF700SA Polypropylene HF700SA is a polypropylene homopolymer intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: household applications.Infor.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.0 °C | 127 °F | ISO 75 |
Unipetrol PP MONSTEN® NB 218 Polypropylene Homopolymer Made for fibers applications. Basic stabilization. Homopolymer.Information provided by Unipetrol RPA |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.0 °C | 127 °F | ISO 75 |
Unipetrol PP MONSTEN® NB 425 Polypropylene Homopolymer Made for non-woven textiles applications. Basic stabilization. Homopolymer.Information provided by Unipetrol RPA |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.0 °C | 127 °F | 120°C per hour; ISO 75-2 |
Total PPC 7612 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 7612 is a nucleated and controlled-rheology heterophasic copolymer. PPC 7612 is characterized by a good balance between rigidity and impact resistance and has excellent antistatic.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.0 °C | 127 °F | 120°C per hour; ISO 75-2 |
Total PPC 7642 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 7642 is a nucleated and antistatic heterophasic copolymer. PPC 7642 is characterized by a very high stiffness. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.0 °C | 127 °F | 120°C per hour; ISO 75-2 |
Total PPC 9642 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 9642 is nucleated heterophasic copolymer. PPC 9642 is characterized by improved stiffness, creep resistance, high impact resistance, excellent antistatic properties and has been f.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.0 °C | 127 °F | ASTM D648 |
A. Schulman POLYPUR™ FPU 1152C Thermoplastic Polyurethane Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.0 °C | 127 °F | ASTM D648 |
A. Schulman POLYPUR™ FPU 1152C Thermoplastic Polyurethane Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.0 - 54.0 °C | 127 - 129 °F | ASTM D648-98c |
DSM Somos® ProtoGen™ O-XT 18420 Epoxy Resin for Stereolithography, UV Postcure at HOC +3 DescriptionDSM Somos® ProtoGen O-XT 18420 is a liquid, ABS-like, photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demons.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.8 °C | 127 °F | ISO 75-2/A |
ExxonMobil PP4031E2 Polypropylene Impact Copolymer Product Description: An impact copolymer resin for extrusion applications with high melt viscosity and excellent rigidity, shock resistance and dimensional stability. It is designed for corrugated .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.0 °C | 127 °F | ASTM-D648 |
Braskem H 611 HOMO Polypropylene Homopolymer H 611 is a low melt flow rate homopolymer that was specially designed for exposure to solar light. This product exhibits good processability and high melt resistance. It is designed for raffia extru.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.8 °C | 127 °F | |
Aclo Accutech Polypropylene Copolymer CP0437T20L Talc Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.0 °C | 127 °F | ASTM D648 |
Adell BD-30 Nylon 6, Ultra High Impact Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.0 °C | 127 °F | |
BASF Novolen® 2348 M Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.0 °C | 127 °F | ASTM D648 |
Braskem CP 191 Injection Molding Polypropylene Applications: Household; low temperature packing; frozen desserts packaging. Information provided by Braskem |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.0 °C | 127 °F | ISO 75-2/AF |
Addiplast Addilene J 683 Polypropylene Copolymer Copper ResistantInformation provided by Addiplast. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.0 °C | 127 °F | ASTM Data |
BASF Capron® 8351 Impact Modified Nylon 6 (Dry)
(discontinued **) Capron 8351 is a type 6 polyamide graft copolymer developed for injection molding applications requiring a high level of toughness combined with moderate flexibility and faster cycles. It is also .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.0 °C | 127 °F | ASTM D648 |
Braskem H 306 Injection Molding Polypropylene Description: H 306 is a medium melt flow rate additivated homopolymer used for general purposes. It suitable for injection moulding and fiber extrusion. This product exhibits excellent processabilit.. |