Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 45.0 °C | 113 °F | ASTM D648 |
RedEye On Demand VeroBlack PolyJet™ FC870 for Rapid Prototyping Vero PolyJet Resin (VeroBlue™ FC840 & VeroBlack™ FC870) is a photopolymer resin designed for precise jetting in super fine layers by PolyJet™ Technology, often used in rapid prototyping. Our Vero.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 45.0 °C | 113 °F | |
LATI Latiblend 5262 PP Homopolymer/PA6 Blend based on Polypropylene homopolymer (PPh) / Polyamide 6 (PA6). Unfilled. High impact resistance. Very good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 45.0 °C | 113 °F | ISO 75 |
LyondellBasell Hifaxâ„¢ CA187 Thermoplastic Olefin Resin Key Features: medium melt flow, medium modulus, paintable thermoplastic elastomeric olefin resin, excellent paintability, excellent surface appearance, good impact and stiffness balanceApplications:.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 45.0 °C | 113 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP TH0750A PUR (Asia Pacific) LNP THERMOCOMP* TH0750A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 45.0 °C | 113 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® L 16 nat PA12 Low viscosity unmodified polyamide 12Information provided by EMS Grivory |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 45.0 °C | 113 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® L 20 G HL PA12 Product Description: Grilamid L 20 GHL is a, medium viscosity injection molding grade, based on Polyamide 12 (PA12). Grilamid L 20 GHL is UV-stabilized, and heat stabilized The special features of G.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 45.0 °C | 113 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® L 20 GM PA12 Product Description: Grilamid L 20 GM is a medium viscosity, heat stabilized polyamide 12 non-reinforced injection molding grade. This product has very good flow characteristics. Special features of.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 45.0 °C | 113 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® L 20 HL black 9563 PA12 Product Description: Grilamid L 20 HL black 9563 is a, medium viscosity extrusion grade, based on Polyamide 12 (PA12). Grilamid L20 HL black 9563 has been especially developed for external cable she.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 45.0 °C | 113 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® L 20A Z PA12 Product Description: Grilamid L 20A Z is a medium viscosity product, based on Polyamide 12 (PA12). Grilamid L 20A Z is impact modified, hydrolysis-and heat stabilized. Grilamid L 20A Z is used for p.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 45.0 °C | 113 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® L 20H FWA black 9225 PA12 Product Description Grilamid L 20 H FWA black 9225 is a medium viscosity, unreinforced and heat stabilized Polyamide 12 (PA12). Grilamid L 20 H FWA black 9225 is used for technical injection molded .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 45.0 °C | 113 °F | ISO 75-2/A |
ExxonMobil Exxtral™ BNU 013 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good impact resistance, high stiffness, good scratch and good surface finishing designed for automotive interior ap.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 45.0 °C | 113 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® L 25 nat 6112 PA12 Product Description: Grilamid L 25 natural 6112 is a high viscous, Polyamide 12 extrusion grade. Grilamid L 25 natural 6112 fulfils the requirements of DIN 73378, Type PA 12-H. Application examples:.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 45.0 °C | 113 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® L 25 W 20 Y PA12-I Product Description: Grilamid L 25 W 20 Y black 9992 is a semiflexible plasticized, medium viscosity, extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 20 Y black 9992 is impact modified, heat.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 45.0 °C | 113 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® L 25H FWA black 9225 PA12 Product Description: Grilamid L 25 H FWA black 9225 is a highviscosity, unreinforced and heat stabilized Polyamide 12 (PA12). Grilamid L 25 H FWA black 9225 is designed for technical injection mould.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 45.0 °C | 113 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® L 25H FWA nat PA12 Product Description: Grilamid L 25 H FWA natural is a highviscosity, unreinforced and heat stabilized Polyamide 12 (PA12). Grilamid L 25 H FWA natural is designed for technical injection moulded com.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 45.0 °C | 113 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® R 50 H NZ PA6 Product description: Grilon R 50 H NZ is a high viscosity, unreinforced, heat stabilized, impact modified PA6 extrusion blow molding grade. Grilon R 50 H NZ has the following important properties: V.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 45.0 °C | 113 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® ST7301 BK356 Nylon 6
(Unverified Data**) Super Toughened Polyamide 6 Zytel ST7301 BK356 is a Super Tough heat stabilized lubricated black polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 45.0 °C | 113 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® L 25 H PA12 Product Description: Grilamid L 25 H is a high viscosity heat stabilized Polyamide 12 extrusion grade and is suitable for application requiring a long-term usage temperature of 100 - 120°C. The mai.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 45.0 °C | 113 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® L 25 W 40 ESD PA12 Product Description: Grilamid L 25 W 40 ESD is a high viscosity, anti-static highly flexible extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 40 ESD is plasticized and heat stabilized The inh.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 45.0 °C | 113 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® L 25 W 40 HL X PA12-I Product Description: Grilamid L 25 W 40 HLX is a flexible Polyamide 12 grade with an excellent cold impact strength and heat stability. Grilamid L 25 W 40 HLX is specially suitable for flexible tube.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 45.0 °C | 113 °F | ISO R75 |
Arkema Group Orgalloy® LE 6000 Polyamide 6 Alloy Polyamide Alloy, Semi-Flexible grade, Nylon 6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 45.0 °C | 113 °F | |
Arkema Group Rilsan® BMN P40 D Nylon 11 (Conditioned) Designation ISO 1874-PA11-P,MR,12-003Flexible grade for injection molding. Available colors: black, natural and white. Mold release agent.Flexibility. Outstanding working properties. Easy filling of.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 45.0 °C | 113 °F | cond.; ISO 75 |
Azoty Tarnow™ Tarnamid® T-27 MCS HI Polyamide 6 - Impact Modified Very high impact resistance, cold impact grade (to -40°C). Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has t.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 45.0 °C | 113 °F | |
Covestro Texin® 970U Urethane Thermoplastic Elastomer Key Features:UnfilledU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingProfile extrusionSheet extrusionInformation provided by Bayer Polymers.As of 1 September 2015, B.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 45.0 °C | 113 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® BR 40 W PA6 Product description: Grilon BR 40 W is a medium viscosity, plasticized PA6 extrusion grade. Grilon BR 40 W has the following important properties: High flexibilityHigh stiffness Grilon BR 40 W is us.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-07 |
Proto3000 Objet VeroWhitePlus FullCure835 Rigid Opaque Prototyping Polymer Information provided by Proto3000 for their protoyping engineering services. |