Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 127 - 235 °C | 261 - 455 °F | Average value: 178 °C Grade Count:5 |
Overview of materials for Nylon 66/6, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 125 - 235 °C | 257 - 455 °F | Average value: 150 °C Grade Count:23 |
Overview of materials for Polyphenylene Ether, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu.. |